| Part NO. | AWG | Standard Length | Weight | Meas. (cm*cm*cm) | ||
| ft./reel | ft./CTN | N.W.(kgs) | G.W.(kgs) | |||
| AT | 8 | 500 | 500 | 39 | 41 | 41.5*41.5*20 |
| AT | 10 | 500 | 500 | 22 | 23 | 30.5*30.5*23 |
| AT | 12 | 500 | 500 | 16 | 17 | 30.5*30.5*19 |
| AT | 14 | 500 | 500 | 14 | 15 | 30.5*30.5*18 |
| AT | 16 | 500 | 1000 | 20 | 21 | 30.5*30.5*23 |
Main Technical Data
| Max.d.c. resistance of conductor ( | Min.d.c. resistance of insulation ( |
| 9.2 | 15 |
| 5.4 | 15 |
| 4.1 | 15 |
| 2.6 | 15 |
Capability of Sheath
| Capability of insulating layer | Reference value |
| Tensile strength: ≥MPa | 10.3 |
| Elongation at break: ≥% | 100 |
| Cold bending: ℃*h | -160 |
| Combustion experiment: | FT2 |
| Ageing temperature: ℃ | 136±2 |
| Ageing time: h | 168 |
| Percent retention of tensile strength: ≥% | 85 |
| Percent retention of extensibility: ≥% | 65 |
| Temperature of oil resistant experiment: ℃ | 60 |
| Time of oil resistant experiment: h | 168 |
| Percent retention of tensile strength: ≥% | 75 |
| Percent retention of extensibility: ≥% | 75 |
| Time of carbon arc and xenon arc experiment : h | 72 |
| Percent retention of tensile strength: ≥% | 80 |
| Percent retention of extensibility: ≥% | 80 |